BioLever Mini; small nitride cantilever with silicon tip for tapping mode in liquid.
f = 110 kHz | k = 0.09 N/m | tip coating: none
Also known as OTESPA; silicon probe with visible apex tip for tapping mode.
f = 300 kHz | k = 26 N/m | tip coating: none
BioLever fast (also known as BL-AC10DS); ultra small cantilever for tapping mode in liquid.
Only on AFMs with
small laser spot such as Cypher.
f = 1500 kHz | k = 0.1 N/m | tip coating: none
Asylum electrolever with visible tip apex and conductive coating for nano-electrical measurements
f = 75 kHz | k = 2.8 N/m | tip coating: Ti/Ir
Silicon probe with visible apex tip for force modulation or soft tapping on medium to hard samples.
f = 150 kHz | k =9 N/m | tip coating: none
Also known as OLTESPA; medium soft cantilever for topgraphy and viscoelasticity of soft samples.
f = 70 kHz | k = 2 N/m | tip coating: none
Silicon probe with visible tip apex and magnetic coating for low coercivity MFM applications.
f = 75 kHz | k = 2.8 N/m | tip coating: permalloy
OLTESPA with Au reflective coating; medium soft cantilever for topography and viscoelasticity of soft samples.
f = 70 kHz | k = 2 N/m | tip coating: none
Sharp conductive probe with PtSi coating for electrical measurements.
f = 75 kHz | k = 2.8 N/m | tip coating: PtSi
Asylum electrolever with visible tip apex and conductive coating for tapping/non-contact mode.
f = 300 kHz | k = 42 N/m | tip coating: Ti/Ir
Silicon probe with visible tip apex and magnetic coating for standard MFM applications.
f = 75 kHz | k = 2.8 N/m | tip coating: CoCr
Silicon probe with visible tip apex and magnetic coating for low moment MFM applications.
f = 75 kHz | k = 2.8 N/m | tip coating: CoCr
OTESPA with Au reflective coating; silicon probe with visible apex tip for tapping mode.
f = 300 kHz | k = 26 N/m | tip coating: none
Silicon probe with visible tip apex and magnetic coating for high coercivity MFM applications.
f = 75 kHz | k = 2.8 N/m | tip coating: CoPt/FePt
BioLever fast with CNF tips (also known as BL-AC10FS); Carbon Nano Fiber probe for high resolution imaging.
Only on AFMs with
small laser spot such as Cypher.
f = 1500 kHz | k = 0.1 N/m | tip coating: none
Silicon probe with visible tip apex and magnetic coating for high moment MFM applications.
f = 75 kHz | k = 2.8 N/m | tip coating: CoCr
Silicon probe with visible tip apex and Au reflex coating for high speed imaging.
f = 2000 kHz | tip coating: none
Also known as OSCM; conductive probe with visible apex tip for electrical measurement.
f = 70 kHz | k = 2 N/m | tip coating: Ti/Pt
Fast silicon probe with visible apex tip for fast imaging.
Only on AFMs with
small laser spot such as Cypher.
f = 1600 kHz | k = 85 N/m | tip coating: none
Asylum electrolever with visible tip apex and conductive coating for tapping/non-contact mode.
f = 285 kHz | k = 42 N/m | tip coating: Ti/Ir
Silicon probe with Al reflective coating for soft tapping mode.
f = 160 kHz | k = 7.4 N/m | tip coating: none
Silicon probe with PtIr coating for tapping/non-contact mode.
f = 320 kHz | k = 42 N/m | tip coating: Pt/Ir
Silicon probe with Al reflex coating for force modulation mode.
f = 75 kHz | k = 2.8 N/m | tip coating: none
Silicon probe coated with high moment material for MFM.
f = 75 kHz | k = 2.8 N/m | tip coating: hard magnetic
Five each of Asylum MFM levers (ASYMFM; ASYMFMHC-R2; ASYMFMHM; ASYMFMLC; ASYMFMLM); Veeco equiv - MESPSP
Conductive probe for electrical measurements in force modulation mode.
f = 75 kHz | k = 2.8 N/m | tip coating: Pt/Ir
Nitride probe with shielded co-axial sensor specialized for sMIM applications.
f = 75 kHz | k = 8 N/m | tip coating: TiW/Au
Silicon probe with Al reflex coating for soft tapping mode.
f = 160 kHz | k = 7.4 N/m | tip coating: none
Silicon probe with PtIr coating for force modulation.
f = 75 kHz | k = 2.8 N/m | tip coating: Pt/Ir
Silicon probe with sharp tip for high resolution imaging in force modulation mode.
f = 75 kHz | k = 2.8 N/m | tip coating: none
Silicon probe with Au reflex coating for tapping/non contact mode.
f = 330 kHz | k = 42 N/m | tip coating: none
Nitride probe with shielded co-axial sensor specialized for sMIM applications.
f = 19 kHz | k = 1 N/m | tip coating: TiW/Au
Conductive probe with visible tip apex for electrical measurements in modulation mode.
f = 85 kHz | k = 2.8 N/m | tip coating: Pt/Ir
Silicon probe coated with thin magnetic material for high resolution MFM.
f = 75 kHz | k = 2.8 N/m | tip coating: hard magnetic
Quartz-like material probe with carbon EBD tip for high speed imaging in tapping/non-contact mode.
To be used only on AFMs with
small laser spot
f = 2000 kHz | k = 3 N/m | tip coating: none
Nitride probe with two triangular cantilevers for iDrive mode.
f = 10 & 32 kHz | k =0.02 & 0.09 N/m | tip coating: Cr/Au
CoNi side-coated tip silicon probe for high hi-resolution MFM.
f = 75 kHz | k = 2.8 N/m | tip coating: CoNi
Silicon probe with sharp tip for high resolution imaging in tapping/non-contact mode.
f = 330 kHz | k = 42 N/m | tip coating: none
Silicon probe with Al reflex coating for tapping/non-contact mode.
f = 320 kHz | k = 42 N/m | tip coating: none
Silicon probe with Al reflex coating for contact mode.
f = 13 kHz | k = 0.2 N/m | tip coating: none
Silicon probe with conductive diamond coated tip for electrical measurements.
f = 400 kHz | k = 80 N/m | tip coating: conductive diamond
Silicon probe coated with low coercivity material for MFM on soft magnetic samples.
f = 75 kHz | k = 2.8 N/m | tip coating: soft magnetic
Quartz-like material probe with carbon EBD tip for high speed imaging in tapping/non-contact mode.
To be used only on AFMs with
small laser spot
f = 300 kHz | k = 0.3 N/m | tip coating: none
Conductive silicon probe with Au tip coating for electrical measurements in non-contact/tapping mode.
f = 330 kHz | k = 42 N/m | tip coating: Au
Silicon probe with short cantilever and Au reflective coating for contact mode.
f = 23 kHz | k = 0.2 N/m | tip coating: none
Silicon probe with high aspect ratio tip (>5) for deep trench imaging.
f = 330 kHz | k = 42 N/m | tip coating: none
Quartz-like material probe with carbon EBD tip for high speed imaging in tapping/non-contact mode.
To be used only on AFMs with
small laser spot
f = 5000 kHz | k = 30 N/m | tip coating: none
Silicon probe with Au reflective coating for soft tapping mode.
f = 160 kHz | k = 7.4 N/m | tip coating: none
Silicon probe with long cantilevr and Au reflective coating for tapping/non contact mode.
f = 190 kHz | k = 48 N/m | tip coating: none
Nanoworld silicon probe with conductive diamond coating for tapping/non-contact mode.
f = 400 kHz | k = 80 N/m | tip coating: conductive diamond